Sciweavers
Explore
Publications
Books
Software
Tutorials
Presentations
Lectures Notes
Datasets
Labs
Conferences
Community
Upcoming
Conferences
Top Ranked Papers
Most Viewed Conferences
Conferences by Acronym
Conferences by Subject
Conferences by Year
Tools
Sci2ools
International Keyboard
Graphical Social Symbols
CSS3 Style Generator
OCR
Web Page to Image
Web Page to PDF
Merge PDF
Split PDF
Latex Equation Editor
Extract Images from PDF
Convert JPEG to PS
Convert Latex to Word
Convert Word to PDF
Image Converter
PDF Converter
Community
Sciweavers
About
Terms of Use
Privacy Policy
Cookies
20
click to vote
CVPR
2011
IEEE
396
views
Computer Vision
»
more
CVPR 2011
»
A Multichannel Edge-Weighted Centroidal Voronoi Tessellation Algorithm for 3D Superalloy Image Segmentation
13 years 10 days ago
Download
www.cse.sc.edu
In material science and engineering, the grain structure inside a super-alloy sample determines its mechanical and physical properties. In this paper, we develop a new Multichannel...
Y. Cao, L. Ju, Q. Zou, C. Qu, S. Wang